RUBBER COMPOSITION AND PNEUMATIC TIRE

A rubber composition is disclosed comprising, based on 100 parts by weight of elastomer (phr),(A) from 30 to 50 phr of a first solution polymerized styrene-butadiene rubber having a glass transition temperature (Tg) in a range of from -80 °C to -50 °C and functionalized with an alkoxysilane group an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NZULU, Frida, POMPEI, Manuela, STEINER, Pascal Patrick, DELVILLE, Jerome Joel Daniel
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A rubber composition is disclosed comprising, based on 100 parts by weight of elastomer (phr),(A) from 30 to 50 phr of a first solution polymerized styrene-butadiene rubber having a glass transition temperature (Tg) in a range of from -80 °C to -50 °C and functionalized with an alkoxysilane group and at least one functional group selected from the group consisting of primary amines and thiols;(B) from 30 to 50 phr of a second solution polymerized styrene-butadiene rubber having a glass transition temperature (Tg) in a range of from -40 °C to -10 °C and functionalized with an alkoxysilane group and at least one functional group selected from the group consisting of primary amines and thiols;(C) from 0 to 40 phr of a polyisoprene having a cis 1,4 content greater than 95 percent selected from the group consisting of natural rubber and synthetic polyisoprene;(D) from 20 to 60 phr of a hydrocarbon resin having a Tg of at least 30°C;(E) from 40 to 80 phr of an oil; and(F) from 120 to 180 phr of silica.The rubber composition is for use in a tread of a pneumatic tire.