CEMENTED CARBIDE AND ITS PRODUCTION METHOD, AND ROLLING ROLL
A cemented carbide comprising 55-90 parts by mass of WC particles, and 10-45 parts by mass of an Fe-based binder phase, the binder phase having a composition comprising 2.5-10% by mass of Ni, 0.2-1.2% by mass of C, 0.5-5% by mass of Cr, 0.2-2.0% by mass of Si, 0.1-3% by mass of W, 0-5% by mass of Co...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A cemented carbide comprising 55-90 parts by mass of WC particles, and 10-45 parts by mass of an Fe-based binder phase, the binder phase having a composition comprising 2.5-10% by mass of Ni, 0.2-1.2% by mass of C, 0.5-5% by mass of Cr, 0.2-2.0% by mass of Si, 0.1-3% by mass of W, 0-5% by mass of Co, and 0-1% by mass of Mn, the balance being substantially Fe and inevitable impurities, and the cemented carbide being substantially free from composite carbides having major axes of 5 µm or more. This cemented carbide is produced by cooling at a cooling rate of 60°C/hour or more between 900°C and 600°C, after vacuum sintering. |
---|