FERRITIC-AUSTENITIC TWO-PHASE STAINLESS STEEL MATERIAL AND METHOD FOR MANUFACTURING SAME
A steel material contains, in mass%, C: 0.005 to 0.050, N: 0.05 to 0.30, Si: 0.1 to 1.5, Mn: 0.1 to 7.0, P: 0.005 to 0.100, S: 0.0001 to 0.0200, Cr: 18.0 to 28.0, Cu: 0.1 to 3.0, Ni: 0.1 to 8.0, Mo: 0.1 to 5.0, Al: 0.001 to 0.050, B: 0.0001 to 0.0200, and Ca: 0.0001 to 0.0100. An area ratio of an au...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A steel material contains, in mass%, C: 0.005 to 0.050, N: 0.05 to 0.30, Si: 0.1 to 1.5, Mn: 0.1 to 7.0, P: 0.005 to 0.100, S: 0.0001 to 0.0200, Cr: 18.0 to 28.0, Cu: 0.1 to 3.0, Ni: 0.1 to 8.0, Mo: 0.1 to 5.0, Al: 0.001 to 0.050, B: 0.0001 to 0.0200, and Ca: 0.0001 to 0.0100. An area ratio of an austenitic phase ranges from 30% to 70% and formulae (I) and (II) below are satisfied. 1.03 ¤ % Cr * F / % Cr ¤ 1.40 1.05 ¤ % Mn * A / % Mn ¤ 1.80
[% symbol of an element]: a content of the element in the steel
[% symbol of an element*F]: a content of the element in a ferrite phase
[% symbol of element*A]: a content of the element in the austenitic phase |
---|