FLUORINATED TIN-BASED GLASS FRIT AND METHOD FOR MANUFACTURING SAME
Provided is a super low melting SnO-SnF2-P2O5-based glass frit for which the firing temperature can be set to 200°C or less and which has high water resistance and transparency. The fluorinated tin-based glass frit includes, in mol%, 30 to 70% of SnF2, 10 to 30% of P205, 10 to 40% of SnO, 0.1 to 10%...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Provided is a super low melting SnO-SnF2-P2O5-based glass frit for which the firing temperature can be set to 200°C or less and which has high water resistance and transparency. The fluorinated tin-based glass frit includes, in mol%, 30 to 70% of SnF2, 10 to 30% of P205, 10 to 40% of SnO, 0.1 to 10% of SnO2, 0 to 5% of In203, 0 to 5% of B2O3, and 0 to 5% of SiO2, and has a glass transition point of 160°C or lower, a softening point of 180°C or lower, and a maximum particle size of 100 µm or less. The fluorinated tin-based glass frit has a visible light transmission rate of 80% or more at 200°C and a thickness of 0.6 mm of a fired product thereof, and a rate of volume reduction of the fired product due to soaking in hot water at 85°C for 24 hours is 2 vol.% or less. |
---|