A PROCESS FOR PRODUCING AN ETHYLENE-BASED POLYMER

Ethylene-based polymers comprising the following properties: (A) a density less than 0.9190 g/cc; (B) a hexane extractable level that meets the following equation: hexane extractable level ≤A+B [log(12)], where A=2.65 wt %, and B-0.25 wt %[log (dg/min)]; based on total weight of the ethylene-based p...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OSBY, John, O, DEN DOELDER, Cornelis, F.J, HINRICHS, Stefan, KARJALA, Teresa, P, BERBEE, Otto
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ethylene-based polymers comprising the following properties: (A) a density less than 0.9190 g/cc; (B) a hexane extractable level that meets the following equation: hexane extractable level ≤A+B [log(12)], where A=2.65 wt %, and B-0.25 wt %[log (dg/min)]; based on total weight of the ethylene-based polymer; (C) a G′ (at G″=500 Pa, 1 70° C.) that meets the following equation: G′≥C+D [log(12)], where C=150 Pa, and D=−60 Pa/[log(dg/min)]; and (D) a melt index (12) from 0.7 to 20 dg/min; are made in high pressure tubular process that comprises at least three reaction zones with the peak polymerization temperature of the first reaction zone ≥320° C. and the peak polymerization temperature of the last reaction zone ≤290° C.