METHOD FOR PRODUCING AN OPAQUE QUARTZ GLASS CONTAINING PORES
A method for producing a pore-containing opaque quartz glass includes: (a) producing porous SiO2 granulate particles from synthetically produced SiO2, (b) thermally densifying the SiO2 granulate particles to form partly densified SiO2 granulate particles, (c) forming a dispersion from the partly den...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for producing a pore-containing opaque quartz glass includes: (a) producing porous SiO2 granulate particles from synthetically produced SiO2, (b) thermally densifying the SiO2 granulate particles to form partly densified SiO2 granulate particles, (c) forming a dispersion from the partly densified SiO2 granulate particles, (d) comminuting the partly densified SiO2 granulate particles to form a slip containing comminuted SiO2 granulate particles, (e) shaping the slip into a shaped body and forming a porous SiO2 green body with a green density rG, and (f) sintering the SiO2 green body into opaque quartz glass. To produce opaque quartz glass that is also suited for the use of spray granulate, during step (b), partly densified SiO2 granulate particles are produced with a specific surface BET-(A) between 0.025 and 2.5 m2/g, and during step (d), comminuted SiO2 granulate particles are produced with a specific surface BET-(B) between 4 and 10 m2/g. |
---|