METHOD FOR THE CONTINUOUS PRODUCTION OF A LOW-DENSITY MINERAL FOAM
A method for the continuous production of a mineral foam of which the density in the dry state (d) is from 40 to 600 kg/m3, includes (i) mixing cement; a water reducing agent; 0.5 to 10%, % by weight with respect to the total weight of cement, of ultrafine particles having a liquid-solid contact ang...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for the continuous production of a mineral foam of which the density in the dry state (d) is from 40 to 600 kg/m3, includes (i) mixing cement; a water reducing agent; 0.5 to 10%, % by weight with respect to the total weight of cement, of ultrafine particles having a liquid-solid contact angle comprised from 30° to 140°, and of which the D50 is from 10 to 600 nm; water, with a water/cement weight ratio from 0.3 to 2.5; (ii) adding to the mixture from 0.5 to 10% of a pore-forming agent, % by weight with respect to the weight of cement; (iii) applying the mixture obtained at step (ii) on a support; (iv) leaving the mixture to expand on the support. |
---|