POWDER CORE, POWDER CORE MANUFACTURING METHOD, AND METHOD FOR ESTIMATING EDDY CURRENT LOSS IN POWDER CORE

An eddy current loss at a frequency of 3,000 Hz is set to less than 150 W/kg by setting a single particle diameter-equivalent diameter d s of soft magnetic metal powder represented by the following formula to 210 µm or less. In the formula, d s represents a single particle diameter-equivalent diamet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIMAZU, EIICHIRUO, MUNEDA, NORIKAZU, ARAKI, HIKARU
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An eddy current loss at a frequency of 3,000 Hz is set to less than 150 W/kg by setting a single particle diameter-equivalent diameter d s of soft magnetic metal powder represented by the following formula to 210 µm or less. In the formula, d s represents a single particle diameter-equivalent diameter of the soft magnetic metal powder [m], d MN represents a number average particle diameter of the soft magnetic metal powder [m], and à represents a standard deviation of the particle diameter of the soft magnetic metal powder [m]. d S = d M N 2 + 5 ¢ à 2 + 2 ¢ à 2 ¢ d M N 2 d M N 2 + 3 ¢ à 2