STEEL OIL WELL PIPE HAVING EXCELLENT SULFIDE STRESS CRACKING RESISTANCE
To provide an oil-well steel pipe having excellent SSC resistance. The oil-well steel pipe according to the present invention contains, by mass percent, C: 0.15 to 0.35%, Si: 0.1 to 0.75%, Mn: 0.1 to 1.0%, Cr: 0.1 to 1.7%, Mo: 0.1 to 1.2%, Ti: 0.01 to 0.05%, Nb: 0.010 to 0.030%, Al: 0.01 to 0.1%, P:...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide an oil-well steel pipe having excellent SSC resistance. The oil-well steel pipe according to the present invention contains, by mass percent, C: 0.15 to 0.35%, Si: 0.1 to 0.75%, Mn: 0.1 to 1.0%, Cr: 0.1 to 1.7%, Mo: 0.1 to 1.2%, Ti: 0.01 to 0.05%, Nb: 0.010 to 0.030%, Al: 0.01 to 0.1%, P: at most 0.03%, S: at most 0.01%, N: at most 0.007%, and O: at most 0.01%, the balance being Fe and impurities. The Ti content and the Nb content in a residue obtained by bromine-methanol extraction satisfy equation (1): 100 × Nb / Ti + Nb ‰¤ 27.5
where the Ti content (mass%) and the Nb content (mass%) in the residue are substituted for [Ti] and [Nb]. |
---|