IMPACT-MODIFIED POLYESTER/POLYCARBONATE COMPOSITIONS HAVING IMPROVED ELONGATION AT RUPTURE
The present invention relates to impact-modified polyester/polycarbonate compositions containing: A) 41 to 80 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D, of aromatic polycarbonate, B) 5 to 40 parts by weight, in each case relative to the sum of the...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The present invention relates to impact-modified polyester/polycarbonate compositions containing: A) 41 to 80 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D, of aromatic polycarbonate, B) 5 to 40 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D, of polyester with a content of isophthalic acid building blocks, C) 1 to 15 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D, of rubber-modified graft polymer, D) 0 to 25 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D, of a flame retardant, E) 0 to 20 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D=100, of vinyl (co)polymer, F) 0 to 50 parts by weight, in each case relative to the sum of the parts by weight of components A+B+C+D=100, of additives, wherein all the stated parts by weights in the present application are normalized such that the sum of the parts by weight of components A+B+C+D in the composition amounts to 100, which exhibit improved elongation at break in conjunction with excellent multiaxial toughness and low molding shrinkage. Provided that these compositions have been rendered flame-retardant, they exhibit flame retardant properties which are equal to or better than known compositions. |
---|