METHOD FOR PRODUCING DDR ZEOLITE

Disclosed is a method for producing a DDR zeolite, which can be carried out using materials that are less harmful to the environment. The method for producing a DDR zeolite has a short hydrothermal synthesis time and does not require continuous agitation of the raw material solution. Specifically di...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NIINO, MAKIKO, UCHIKAWA, TETSUYA
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Disclosed is a method for producing a DDR zeolite, which can be carried out using materials that are less harmful to the environment. The method for producing a DDR zeolite has a short hydrothermal synthesis time and does not require continuous agitation of the raw material solution. Specifically disclosed is a method for producing a DDR zeolite, which comprises: a raw material solution preparation step in which a raw material solution that contains 1-adamantaneamine, silica (SiO 2 ) and water at a molar ratio 1-adamantaneamine/SiO 2 of 0.002-0.5 and a molar ratio water/SiO 2 of 10-500 but does not contain ethylenediamine is prepared; and a crystal growth step in which hydrothermal synthesis is carried out while having the raw material solution and a DDR zeolite powder in contact with each other, so that crystals of DDR zeolite are grown using the DDR zeolite powder as a seed crystal.