POLYMER ALLOY, PROCESS FOR PROUCING SAME, AND MOLDED ARTICLE
At least two or more components of thermoplastic resins are compounded by chaotic mixing to form a polymer alloy with a sophisticatedly controlled dispersed phase structure. In the polymer alloy, a dispersed phase having a non-periodic structure with a correlation length of 0.001 µm to 0.5µm and hav...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | At least two or more components of thermoplastic resins are compounded by chaotic mixing to form a polymer alloy with a sophisticatedly controlled dispersed phase structure. In the polymer alloy, a dispersed phase having a non-periodic structure with a correlation length of 0.001 µm to 0.5µm and having a compactness (C) of 0.05 ¤ (C) ¤ 0.8, wherein the compactness (C) can form a molded product that also has transparency while maintaining the original good heat resistance or mechanical properties of the resins blended. A polymer alloy obtained by compounding at least two or more components of immiscible thermoplastic resins, containing a dispersion structure having particles with an average particle size of 0.001 to 1 µm dispersed therein and satisfying 0 < (a)/(b) ¤ 1.5, wherein (a) and (b) represent a peak half width and the maximum wavenumber of the peak, respectively, in a spectrum obtained by plotting scattering intensity against wavenumber of scattered light in scattering measurement can form a molded product that also has transparency while maintaining the original good heat resistance and mechanical properties of the resins blended. |
---|