METHOD FOR PRODUCING FIRED ALUMINUM TITANATE BODY
A process for producing an aluminum titanate-based fired body, comprising a step of firing a shaped body of a starting material mixture containing an aluminum source powder, a titanium source powder and a magnesium source powder, wherein the BET specific surface area of the magnesium source powder i...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A process for producing an aluminum titanate-based fired body, comprising a step of firing a shaped body of a starting material mixture containing an aluminum source powder, a titanium source powder and a magnesium source powder, wherein the BET specific surface area of the magnesium source powder is not less than 2.0 m 2 /g and not more than 30.0 m 2 /g. |
---|