A method of activating an iron Fischer-Tropsch catalyst by introducing an inert gas into a reactor comprising a slurry of the catalyst at a first temperature, increasing the reactor temperature from the first temperature to a second temperature at a first ramp rate, wherein the second temperature is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BENHAM, Charles B, TAYLOR, Jesse, W, ROLFE, Sara L, DEMIREL, Belma, FRAENKEL, Dan, WRIGHT, Harold, A, BLEY, Richard, REJAI, Bahman
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A method of activating an iron Fischer-Tropsch catalyst by introducing an inert gas into a reactor comprising a slurry of the catalyst at a first temperature, increasing the reactor temperature from the first temperature to a second temperature at a first ramp rate, wherein the second temperature is in the range of from about 150° C. to 250° C., introducing synthesis gas having a ratio of H2:CO to the reactor at a space velocity, and increasing the reactor temperature from the second temperature to a third temperature at a second ramp rate, wherein the third temperature is in the range of from about 270° C. to 300° C. The iron Fischer-Tropsch catalyst may be a precipitated unsupported iron catalyst, production of which is also provided.