CAST SLAB OF NON-ORIENTED MAGNETIC STEEL AND METHOD FOR PRODUCING THE SAME
There is produced a molten steel containing, in mass%, Si: not less than 0.1% nor more than 7.0%, Mn: 0.1% or more, Al: not less than 0.2% nor more than 5.0%, Cr: not less than 0.1% nor more than 10%, and the like, and a balance composed of Fe and inevitable impurities. To the molten steel, REM: not...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | There is produced a molten steel containing, in mass%, Si: not less than 0.1% nor more than 7.0%, Mn: 0.1% or more, Al: not less than 0.2% nor more than 5.0%, Cr: not less than 0.1% nor more than 10%, and the like, and a balance composed of Fe and inevitable impurities. To the molten steel, REM: not less than 0.0005% nor more than 0.03% is added. The molten steel to which REM has been added is casted. A cast slab of non-oriented electrical steel is manufactured as above. |
---|