Increasing the cladding-to-core ratio (D/d) of low D/d ratio core rods in optical fiber preforms

An optical fiber preform is fabricated by inserting a number of core body pieces end-to-end inside a glass cylinder, wherein the pieces may have a cladding-to-core diameter (D/d) ratio within the range of one to four. The cylinder with the inserted core body pieces is mounted vertically on a furnace...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BARISH, ERIC L, WU, FENGQING, FLETCHER III, JOSEPH P
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An optical fiber preform is fabricated by inserting a number of core body pieces end-to-end inside a glass cylinder, wherein the pieces may have a cladding-to-core diameter (D/d) ratio within the range of one to four. The cylinder with the inserted core body pieces is mounted vertically on a furnace and heated so that the cylinder becomes elongated and its outside diameter collapses to form a core rod from which core rod sections with D/d ratios greater than five, can be cut. A soot overcladding is deposited on the circumference of a core rod section until the diameter of the deposited soot builds to a determined value. The core rod section with the deposited soot overcladding is consolidated to obtain a finished optical fiber preform. The preform preferably has a D/d ratio of about 15 or more, and an optical fiber may be drawn directly from the preform.