AGGLOMERATED STONE FOR USING IN SHAFT FURNACES, COREX FURNACES OR BLAST FURNACES, METHOD FOR PRODUCING AGGLOMERATED STONES, AND USE OF FINE AND SUPERFINE IRON ORE DUST
Agglomerated stone comprising (wt.%):cement binding agent (6-15), carbon carrier (up to 20), residual and recyclable substances (up to 20), and optionally accelerator (up to 10), remainder iron ore stone in the form of particles of grain size below 3 mm. After 3 days the iron ore has an initial stre...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Agglomerated stone comprising (wt.%):cement binding agent (6-15), carbon carrier (up to 20), residual and recyclable substances (up to 20), and optionally accelerator (up to 10), remainder iron ore stone in the form of particles of grain size below 3 mm. After 3 days the iron ore has an initial strength of at least 5 N/mm2> and after 28 days a cold compression strength of at least 20 N/mm2>. An independent claim is included for a method of preparing the stone as described above by transfer of the composition to a mold and compacting. |
---|