Ethylene-propylene copolymers with an improved shape stability suitable for modifying lubricating oils and process for the preparation thereof

A process is described for the preparation of viscosity index improver (V.I.I.) additives which includes treatment under high shear conditions of a composition comprising (i) one or more EP(D)M polymers and (ii) one or more polyvinylarene/hydrogenated conjugated diene/polyvinylarene block copolymers...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: TANAGLIA, TIZIANO
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process is described for the preparation of viscosity index improver (V.I.I.) additives which includes treatment under high shear conditions of a composition comprising (i) one or more EP(D)M polymers and (ii) one or more polyvinylarene/hydrogenated conjugated diene/polyvinylarene block copolymers, the weight ratio (i)/(ii) ranging from 98:2 to 80:20, preferably from 97:3 to 90:10, the above process being carried out at a temperature ranging from 150°C to 400°C, preferably from 180°C to 320°C.