PROCESS FOR PRODUCING PARTICULATE IRON METAL

The amounts of a CaO-containing substance, an MgO-containing substance, and a SiO2-containing substance, contained in a raw material mixture, are adjusted such that manufacturing operation is performed with the slag basicity (CaO+MgO)/SiO2 of 1.3 to 2.3, and with MgO-concentration of 5 to 13% by mas...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ITO, SHUZO, TSUGE, OSAMU
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The amounts of a CaO-containing substance, an MgO-containing substance, and a SiO2-containing substance, contained in a raw material mixture, are adjusted such that manufacturing operation is performed with the slag basicity (CaO+MgO)/SiO2 of 1.3 to 2.3, and with MgO-concentration of 5 to 13% by mass as to the slag composition, which are dependent upon the concentration of each of CaO, MgO, and SiO2, contained in the raw material mixture. This provides a manufacturing method for high-quality granulated metallic iron with low sulfur concentration, wherein a raw material mixture containing an iron-oxide-containing substance such as iron ore and a carbonaceous reducing agent such as a carbon material are subjected to reducing and melting with a moving hearth-type reducing furnace while suppressing sulfur concentration as much as possible, generated in the granulated metallic iron, particularly due to the carbon material such as coal.