In accordance with an embodiment of the present invention, a method for reducing residual stress in a nickel-base superalloy article comprising about 40-70% of gamma prime phase and having a gamma prime solvus temperature is disclosed. The method comprises the steps of super-solvus heat treating the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Groh, Jon Raymond, Srivatsa, Shesh Krishna
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In accordance with an embodiment of the present invention, a method for reducing residual stress in a nickel-base superalloy article comprising about 40-70% of gamma prime phase and having a gamma prime solvus temperature is disclosed. The method comprises the steps of super-solvus heat treating the superalloy article about 5-40 DEG F (3-22 DEG C) above the gamma prime solvus temperature; and holding at the super-solvus heat treatment temperature for about 0.25-2 hours, wherein the heat-treated superalloy article has reduced residual stress.