COMPOSITION COMPRISING EPDM AND A PARAFFINIC OIL

The invention relates to a composition having a ethylene-propylene-diene rubber component and a Fischer-Tropsch derived process oil. The process oil preferably has a flash point of above 260° C. and an evaporation loss at 107° C. during 22 hours of less than 0.05 wt %.