EXFOLIATION RESISTANT ALUMINIUM-MAGNESIUM ALLOY

Aluminum-magnesium alloy product for welded mechanical construction, having the following composition, in weight percent: Mg 3.5-6.0, Mn 0.4-1.2, Zn 0.4-1.5, Zr 0.25 max., Cr 0.3 max., Ti 0.2 max., Fe 0.5 max., Si 0.5 max., Cu 0.4 max.; one or more selected from the group: Bi 0.005-0.1, Pb 0.005-0.1...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SAMPATH, DESIKAN, HASZLER, ALFRED, JOHANN, PETER
Format: Patent
Sprache:eng ; fre ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Aluminum-magnesium alloy product for welded mechanical construction, having the following composition, in weight percent: Mg 3.5-6.0, Mn 0.4-1.2, Zn 0.4-1.5, Zr 0.25 max., Cr 0.3 max., Ti 0.2 max., Fe 0.5 max., Si 0.5 max., Cu 0.4 max.; one or more selected from the group: Bi 0.005-0.1, Pb 0.005-0.1, Sn 0.01-0.1, Ag 0.01-0.5, Sc 0.01-0.5, Li 0.01-0.5, V 0.01-0.3, Ce 0.01-0.3, Y 0.01-0.3, and Ni 0.01-0.3; others (each) 0.05 max., (total) 0.15 max.; and balance aluminum.