Paint material for constructional finishing and panel for constructional finishing and method of preparing these
Dried shirasu A is used in its unprocessed original form as a component and 50 to 65% of the dried shirasu A, 30 to 40% of a binding agent B, 3 to 10% of a clay material C, 5 to 10% of shirasu balloons D, 0.08 to 2% of a bond reinforcing agent E, 0.1 to 3% of a color pigment F, and 1 to 5% of fibers...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Dried shirasu A is used in its unprocessed original form as a component and 50 to 65% of the dried shirasu A, 30 to 40% of a binding agent B, 3 to 10% of a clay material C, 5 to 10% of shirasu balloons D, 0.08 to 2% of a bond reinforcing agent E, 0.1 to 3% of a color pigment F, and 1 to 5% of fibers for plaster G are incorporated to prepare a paint material for constructional finishing 1. Furthermore, an appropriate amount of water is added to the paint material for constructional finishing 1 and mixed together. The resulting mixture is applied onto a substrate, such as a gypsum board, veneer plywood, concrete board, mortar-applied waterproof plywood, or asbestos board, and the resulting board is subjected to surface-finishing treatment according to an intended design to prepare a panel for constructional finishing 3. |
---|