Flameproof thermoplastic resin composition
A flameproof thermoplastic resin composition of the present invention comprises (A) 40 to 95 parts by weight of a rubber modified styrene-containing resin composed of (a1) 20 to 100% by weight of a styrene-containing graft copolymer resin containing 18 to 50% by weight of acrylonitrile in the copoly...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A flameproof thermoplastic resin composition of the present invention comprises (A) 40 to 95 parts by weight of a rubber modified styrene-containing resin composed of (a1) 20 to 100% by weight of a styrene-containing graft copolymer resin containing 18 to 50% by weight of acrylonitrile in the copolymer excluding rubber and (a2) 0 to 80% by weight of a styrene-containing copolymer containing 18 to 50% by weight of acrylonitrile; (B) 5 to 60 parts by weight of a polyphenylene ether resin; (C) 2 to 40 parts by weight of a styrene-containing copolymer or a styrene-containing graft copolymer, which uses optionally to 60% by weight of rubber, containing 5 to 18% by weight of acrylonitrile in the copolymer excluding the rubber, per 100 parts by weight of the sum of (A) and (B); and (D) 5 to 30 parts by weight of an aromatic phosphoric acid ester per 100 parts by weight of the sum of (A) and (B). The flameproof thermoplastic resin composition may further comprises 0 to 50 parts by weight of an anti-dripping agent, an impact modifier, a plasticizer, a heat stabilizer, an oxidation inhibitor, a light stabilizer, a compatibilizer, a pigment, a dye and/or an inorganic filler on the basis of 100 parts by weight of the base resin. |
---|