PROCESSES FOR PRODUCING COPOLYMERS OF ETHYLENE AND AT LEAST ONE OTHER OLEFIN
Disclosed herein are ethylene polymers having a density of 0.95 to 0.955, a melt index from 0.2 to 0.6 g/10 min., a high load melt index from 20 to 70 g/10 min., and a heterogeneity index from 10 to 16, and methods of preparing the same. In certain embodiments the polymers can have a shear ratio fro...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Disclosed herein are ethylene polymers having a density of 0.95 to 0.955, a melt index from 0.2 to 0.6 g/10 min., a high load melt index from 20 to 70 g/10 min., and a heterogeneity index from 10 to 16, and methods of preparing the same. In certain embodiments the polymers can have a shear ratio from 65 to 100. |
---|