Process for catalytically splitting carbonaceous material during gasification at 700-1200 (preferably 850-950) degrees C comprises using a fluidized bed made up of particles selected from oxides, hydroxides and carbonates of calcium, aluminum, silicon, nickel, titanium, iron, cobalt, and molybdenum...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Process for catalytically splitting carbonaceous material during gasification at 700-1200 (preferably 850-950) degrees C comprises using a fluidized bed made up of particles selected from oxides, hydroxides and carbonates of calcium, aluminum, silicon, nickel, titanium, iron, cobalt, and molybdenum in a stoichiometric excess. |
---|