Method of manufacturing a ceramic coating
A ceramic layer is produced using precursors dissolved in a formic, acetic or propionic acid solvent. A ceramic layer is produced, using precursors dissolved in a solvent of an organic acid of formula CnH2n+1COOH (n = 0, 1 or 2) and optionally water, by application to a substrate and heating. Prefer...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A ceramic layer is produced using precursors dissolved in a formic, acetic or propionic acid solvent. A ceramic layer is produced, using precursors dissolved in a solvent of an organic acid of formula CnH2n+1COOH (n = 0, 1 or 2) and optionally water, by application to a substrate and heating. Preferred Feature: A strontium-bismuth tantalate layer is formed using a solution of Bi(OAc)3 and Sr(OAc)2 in acetic acid which is heated to above the melting point of a tantalum-containing precursor before mixing with the tantalum-containing precursor in the liquid state. |
---|