Steam reforming catalyst
A steam reforming process is improved by the use of a catalyst comprising a porous aluminum oxide having a pore volume of pores having a pore diameter ranging from 0.1 to 0.5 micron of not less than 0.2 ml/g and a pore volume of pores having a pore diameter of more than 0.5 micron but not more than...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A steam reforming process is improved by the use of a catalyst comprising a porous aluminum oxide having a pore volume of pores having a pore diameter ranging from 0.1 to 0.5 micron of not less than 0.2 ml/g and a pore volume of pores having a pore diameter of more than 0.5 micron but not more than 10 microns of not less than 0.05 ml/g and a purity determined upon ignition dryness of not less than 98% by weight, and nickel in an amount of 3 to 20% by weight in terms of nickel oxide based on the total weight of the catalyst, said catalyst being formed by impregnating said porous aluminum oxide with a solution containing nickel, drying the impregnated aluminum oxide and then calcining the dried aluminum oxide. |
---|