A method for stabilizing hydroisomerates
A method is described for rendering total liquid product hydroisomerates daylight stable and improving their oxidation stability, which method involves treating the hydroisomerate total liquid product (6) with a Group VIII metal on refractory metal oxide catalyst or Group VIII metal on halogenated r...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; fre ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method is described for rendering total liquid product hydroisomerates daylight stable and improving their oxidation stability, which method involves treating the hydroisomerate total liquid product (6) with a Group VIII metal on refractory metal oxide catalyst or Group VIII metal on halogenated refractory metal oxide catalyst under mild conditions (7), which conditions are a temperature in the range of 170 to 270 DEG C, a pressure in the range of 300 to 1500 psi (3.4 to 6.9 MPa) H2, 0.25 to 10 v/v/hr and 500 to 10,000 SCF/B (178 to 890 liters H2/liter oil) H2. |
---|