BATH FOR THE GALVANIC DEPOSITION OF GOLD-TIN ALLOY COATINGS
To produce electrolytic deposition of glossy gold/tin alloys there are employed baths having a pH below 3 which contain 1 to 20 g/l gold in the form of tetracyanoaurate (III), 0.1 to 10 g/l tin, an acid and a conducting salt, whereby the tin is in the form of a tin (IV)-oxalato complex.
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To produce electrolytic deposition of glossy gold/tin alloys there are employed baths having a pH below 3 which contain 1 to 20 g/l gold in the form of tetracyanoaurate (III), 0.1 to 10 g/l tin, an acid and a conducting salt, whereby the tin is in the form of a tin (IV)-oxalato complex. |
---|