Finely divided fuel mixture is obtained by: (a) mixing a base component A made of crushed plastic waste and calcined lime (CaO), the component containing 50 wt. % plastic waste and 3-10 wt. % CaO and water; (b) adding water to the fuel mixture to obtain a final moisture content of 20-30 wt. %; and (...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: ERICH JESSE
Format: Patent
Sprache:est
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Finely divided fuel mixture is obtained by: (a) mixing a base component A made of crushed plastic waste and calcined lime (CaO), the component containing 50 wt. % plastic waste and 3-10 wt. % CaO and water; (b) adding water to the fuel mixture to obtain a final moisture content of 20-30 wt. %; and (c) mixing an additional component of plastic, coal dust, bituminous component, used oil and stearates, which raises the calorific value of the mixture to 11000 KJ/kg. The further component contains iron-containing compounds, e.g. iron oxides, and chips. On mixing the base component A, a final moisture content of 25 wt. % water is obtained. The mixture has a flowable consistency at a particle size of 1-30 (preferably 5-10) mm.