FREMGANGSMÅDE TIL SYREÆTSNING AF EN PHOSPHATKILDE
Process of acid attack with sulphuric acid of a phosphate source comprising calcium or not comprising calcium for a predetermined time period ranging from 20 to 180 minutes in the conditions wherein the molar ratio of sulphate from the sulphuric acid and possibly from the phosphate source to the cal...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | dan |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Process of acid attack with sulphuric acid of a phosphate source comprising calcium or not comprising calcium for a predetermined time period ranging from 20 to 180 minutes in the conditions wherein the molar ratio of sulphate from the sulphuric acid and possibly from the phosphate source to the calcium present in the phosphate source ranges from 0.6 to 0.8, and the content in P2O5 in the attack tank is of less than 6%. |
---|