FREMGANGSMAADE TIL FREMSTILLING AF PAPIR MED STOR TOERSTYRKE OGRINGE VAADSTYRKE

In order to increase the dry strength of paper without at the same time significantly increasing its wet strength, paper is surface-sized with an aqueous solution of an alkali metal salt and/or an alkaline earth metal salt of a copolymer of a) from 90 to 30% by weight of acrylic acid and/or methacry...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GUENDER W, STEDEFEDER J, PFOHL S
Format: Patent
Sprache:dan
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In order to increase the dry strength of paper without at the same time significantly increasing its wet strength, paper is surface-sized with an aqueous solution of an alkali metal salt and/or an alkaline earth metal salt of a copolymer of a) from 90 to 30% by weight of acrylic acid and/or methacrylic acid, and b) from 10 to 70% by weight of acrylonitrile, methacrylonitrile, acrylamide and/or methacrylamide, with or without c) up to 30% by weight of an ester of acrylic acid and/or an ester of methacrylic acid, the copolymer having a viscosity of from 5 to 100 mPas in 2% by weight strength aqueous solution at 20 DEG C, measured in a Brookfield viscometer at 20 revolutions per minute.