VERFAHREN ZUR HERSTELLUNG VON PHENOLHARZSCHAEUMEN UND VON WALZSCHAEUMEN
A method for producing resol type phenol resin foams by blending two resol type phenol resins, a blowing agent and a catalyst. A low molecular weight resol type phenol resin with the number average molecular weight of less than 200 and a high molecular weight resol type phenol resin with the number...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method for producing resol type phenol resin foams by blending two resol type phenol resins, a blowing agent and a catalyst. A low molecular weight resol type phenol resin with the number average molecular weight of less than 200 and a high molecular weight resol type phenol resin with the number average molecular weight of greater than 200 are mixed at a weight ratio of from 5/95 to 80/20 and used as the resol type phenol resin. The resol type phenol resin foams are excellent in adhesion, fire-proofness capable of foaming cure in a short time and useful for sprayed-in-place foaming, etc. The phenol resin foams produced by the invention are capable of integral foaming with rigid urethane resin foam layer into foamed laminates of excellent thermal insulation, fire-proofness, etc. |
---|