Polypropylen Harzmischung
A polypropylene resin composition comprises (A) (a-1) a specific crystalline propylene/ethylene block copolymer or (a-3) a polymer mixture comprising the (a-1) and (a-2) a specific crystalline propylene homopolymer in specific ratio, in an amount of 5 to 56% by weight, (B) a hydroxyl group-containin...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A polypropylene resin composition comprises (A) (a-1) a specific crystalline propylene/ethylene block copolymer or (a-3) a polymer mixture comprising the (a-1) and (a-2) a specific crystalline propylene homopolymer in specific ratio, in an amount of 5 to 56% by weight, (B) a hydroxyl group-containing polypropylene having an intrinsic viscosity Ä eta Ü of 0.8 to 2.0 dl/g and a melting point of 150 to 168 DEG C, in an amount of 10 to 45% by weight, (C) a copolymer rubber of ethylene and an alpha -olefin having a melt flow rate (ASTM D-1238, 230 DEG C, load of 2160 g) of 0.5 to 15 g/10 min, in an amount of 18 to 25% by weight, (D) a hydrogenation product of a block copolymer containing a polymer block of a monovinyl-substituted aromatic hydrocarbon compound and a polymer block of a conjugated diene compound, in an amount of 1 to 10% by weight, and (E) an inorganic filler in an amount of 15 to 25% by weight, the total amount of said components (A), (B), (C), (D) and (E) being 100% by weight, hydroxyl group-containing monomer units derived from the hydroxyl group-containing polypropylene (B) being contained in amounts of 1.3 to 4.0% by weight in 100% by weight of the polypropylene resin composition. The polypropylene resin composition exhibits excellent coating adhesion properties and has excellent processability and mechanical strength with a good balance. |
---|