DE3922508

Method of producing amorphous silicic acid and acid solutions of Al salts consists of decomposing the glassy residue of fossel fuel reactors, pref. melt chamber granulate with hot mineral acids. After stirring, the undissolved residue is sepd. washed and dried to be recovered as silicic acid. The ac...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HUELLER, ROLF. DR., 8712 VOLKACH, DE, HANTSCHEL, PETER-MIN., 3446 MEINHARD, DE
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Method of producing amorphous silicic acid and acid solutions of Al salts consists of decomposing the glassy residue of fossel fuel reactors, pref. melt chamber granulate with hot mineral acids. After stirring, the undissolved residue is sepd. washed and dried to be recovered as silicic acid. The acid solns. is treated to recover the aluminium components. The hot acid is pref. 10-37% HCl or H2SO4 and it is used at between 50 deg.C and its boiling point. The acid solution is cooled and/or neutralised and/or alkali adjusted to bring about precipitation of some materials which together with the remaining soln. are further worked. USE/ADVANTAGE - To recover amorphous silicic acid and aluminium hydroxide and alkali aluminates in technically usable quality. The silicic acid is a starting material for producing synthetic zeolite, filler material and at support for catalsyt.