DE3215120
A shrink film having high optical clarity, good shrink properties, and good mechanical properties is obtained by stretching biaxially a film made of a copolymer of ethylene with at least one C8-C18 alpha -olefin, which copolymer has two distinct crystallite melting points below 128 DEG C, the differ...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A shrink film having high optical clarity, good shrink properties, and good mechanical properties is obtained by stretching biaxially a film made of a copolymer of ethylene with at least one C8-C18 alpha -olefin, which copolymer has two distinct crystallite melting points below 128 DEG C, the difference between these melting points being at least 15 DEG C, and stretching being carried within the temperature range defined by these melting points. The above copolymer may be blended with a homopolymer of ethylene or copolymer of ethylene with an ethylenically unsaturated comonomer, which may constitute up to about 95 weight % of the blend. |
---|