Process for improving the flow properties of polyurethane elastomers

In order to improve the flow properties, thermoplastic polyurethane elastomers having molecular weights of greater than 30,000 at temperatures of 150 to 230 DEG C and shear rates of from 10 to 2,000 sec are treated for from 0.1 to 20 minutes with alcohols, monoamines and/or diamines in amounts of fr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HACKL,CHRISTA, BITTNER,GERHARD,.DR, WERNER,FRANK,.DR, MALTE,.ROMBRECHT,HANS
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:In order to improve the flow properties, thermoplastic polyurethane elastomers having molecular weights of greater than 30,000 at temperatures of 150 to 230 DEG C and shear rates of from 10 to 2,000 sec are treated for from 0.1 to 20 minutes with alcohols, monoamines and/or diamines in amounts of from 0.01 to 10% by weight, based on the weight of the polyurethane elastomers.