VERFAHREN ZUM HERSTELLEN VON EISENPULVER

Iron oxide powder, e.g., ore, is reduced in a CO/N2 atmosphere at a temperature between 750 DEG to 1200 DEG C., whereby prior to the onset of precipitation of metallic iron the content of H2 is limited to 15% (vol) of the CO content, and SO2, H2S, COS or another suitable gaseous sulphur compound is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GREBE, KLAUS.. DR., 4307 KETTWIG, HAAS, HANS DE., 4005 MEERBUSCH
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Iron oxide powder, e.g., ore, is reduced in a CO/N2 atmosphere at a temperature between 750 DEG to 1200 DEG C., whereby prior to the onset of precipitation of metallic iron the content of H2 is limited to 15% (vol) of the CO content, and SO2, H2S, COS or another suitable gaseous sulphur compound is developed or maintained in the reducing atmosphere at a range from 0.0005 to 0.1% (vol), preferably 0.001 to 0.01% (vol) in relation to the CO content.