VERFAHREN UND VORRICHTUNG ZUM EXTRUDIEREN UND ABSCHRECKEN EINER POLYMEREN FOLIE

1469983 Quenching polymeric film IMPERIAL CHEMICAL INDUSTRIES Ltd 9 July 1975 [7 Aug 1974] 34781/74 Heading B5B Polymeric film 4 is extruded on to an electrically earthed moving casting surface 3 of a casting drum 2 rotating in the direction shown by the arrow A at a speed greater than that at which...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ALAN REMMINGTON,TIMOTHY, ROBINSON,WILLIAM
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:1469983 Quenching polymeric film IMPERIAL CHEMICAL INDUSTRIES Ltd 9 July 1975 [7 Aug 1974] 34781/74 Heading B5B Polymeric film 4 is extruded on to an electrically earthed moving casting surface 3 of a casting drum 2 rotating in the direction shown by the arrow A at a speed greater than that at which bubbles can be prevented from being entrapped between the molten film and the surface, e.g. peripheral speeds of 140-240 ft./min., after first passing an electrostatic pinning electrode 7 and a suction knife 10 located on the opposite side from the pinning wire. The pinning wire is insulated over that length not covering the film 4 to prevent sparking. The film is preferably polyethylene terephthalate.