VERFAHREN ZUR HERSTELLUNG VON HARZEN VOM NOVOLAK-TYP, NACH DIESEM VERFAHREN HERGESTELLTE HARZE, SIE ENTHALTENDE LACKE UND MIT DEN HARZEN IMPRAEGNIERTE GEGENSTAENDE

Novolak-type resins are prepared by phenolating a toluene-formaldehyde resin of oxygen content 4 - 18% and the product is reacted with hexamine to give a higher softening point of not less than 60 DEG C. The resins may be dissolved in a solvent to form a varnish; such varnishes can impregnate sheet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GORDON ROBINSON,JOSEPH, ANN BRAIN,SALLY
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Novolak-type resins are prepared by phenolating a toluene-formaldehyde resin of oxygen content 4 - 18% and the product is reacted with hexamine to give a higher softening point of not less than 60 DEG C. The resins may be dissolved in a solvent to form a varnish; such varnishes can impregnate sheet material and laminates of good water resistance and electrical properties can be formed therefrom.