Aluminium recovered as its trichloride - by treatment of ground calcined shales with chlorine contg. gases

Shale contg. is not 30 wt.% ash, of which is not 20% is Al calculated on basis of Al2O3, is ground to e.g. 0.01-0.02 mm, and calcined with simultaneous coking in a reducing atmos. at e.g. 700-800 degrees C. Resulting solid material is treated with gas contg. 1 pt. CO and 1-3 pts. Cl at 700-1000 degr...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NEMECZ, ERNO, UJHIDY, AUREL, SZEPVOLGYI, JANOS, KAPOLYI, LASZLO, SZEKELY, TAMAS, BORLAI, OSZKAR, POLINSZKY, KAROLY
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Shale contg. is not 30 wt.% ash, of which is not 20% is Al calculated on basis of Al2O3, is ground to e.g. 0.01-0.02 mm, and calcined with simultaneous coking in a reducing atmos. at e.g. 700-800 degrees C. Resulting solid material is treated with gas contg. 1 pt. CO and 1-3 pts. Cl at 700-1000 degrees C during e.g. 90 mins. AlCl is recovered from gas phase and corresponds e.g. to 54% conversion of Al content of feed. Ash content of shale is pref. silica clay or esp. calcium pyrites. Shale is esp. "Konststein.".