Solid electrolyte contg alumina, titania and zirconia - used in metallurgy for determining degree of oxidn. of liq. metals e.g. steel

Solid electrolyte contg., by wt., 85-95 % Al2O3, 1-5% TiO2 and 4-10% ZrO2, has raised working life, e.g. to 2-4 hrs. in uninterrupted contact with metal and >80-90% reliability in working. Props. include : 0-1 open porosity, 3.7-4.1 g/cc apparent density, 8-15 temp. change cycle stability at 1300...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SEMKINA GEB. KRASNENKO, NOWELLA W, NETSCHAJEW, EWGENIJ A, MAMAJEWA, GALINA A, WINOGRADOW, WIKTOR P
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Solid electrolyte contg., by wt., 85-95 % Al2O3, 1-5% TiO2 and 4-10% ZrO2, has raised working life, e.g. to 2-4 hrs. in uninterrupted contact with metal and >80-90% reliability in working. Props. include : 0-1 open porosity, 3.7-4.1 g/cc apparent density, 8-15 temp. change cycle stability at 1300-20 degrees C in air, 93-98% ion conductivity.