Low temp sintered formed bodies - based on alkaline earth oxides and oxidic sinter promotors
Alkaline earthed oxides are mixed by addition in soln. in quench soln. plasma torch or electric arc with oxides of Gp III siO2, TiO2 and/or oxides of VI or VII sub-gps. and/or oxides of Co.Ni,Fe or B2O3. or their cpds. which decompose thermally before the sinter temp. is reached, so as to produce a...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Alkaline earthed oxides are mixed by addition in soln. in quench soln. plasma torch or electric arc with oxides of Gp III siO2, TiO2 and/or oxides of VI or VII sub-gps. and/or oxides of Co.Ni,Fe or B2O3. or their cpds. which decompose thermally before the sinter temp. is reached, so as to produce a homogeneous mixt. of additive and alkaline earth oxide during the sinter cycle. |
---|