DE2014391

A process for the preparation of non-pyrophoric nickel skeleton catalysts, in which 30 to 80 percent by weight of metallic zinc, 60 to 20 percent by weight of metallic nickel and 0 to 40 percent by weight of one or more further metals soluble in alkaline solutions are heat-treated at temperatures in...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CSUEROES, ZOLTAN, PETRO, JOZSEF, BEKASSY, SANDOR, MATHE, TIBOR, TUNGLER, ANTAL
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for the preparation of non-pyrophoric nickel skeleton catalysts, in which 30 to 80 percent by weight of metallic zinc, 60 to 20 percent by weight of metallic nickel and 0 to 40 percent by weight of one or more further metals soluble in alkaline solutions are heat-treated at temperatures in the range of 880 DEG to 1,120 DEG C for at least 3 minutes, preferably for 10 to 30 minutes, with simultaneous protection of the surface of the melt against oxidation, the melt thus obtained is cooled at a rate not exceeding 120 DEG /minute in the average, the alloy thus obtained is powdered or granulated, and the powdered or granulated alloy is treated with an alkali hydroxide solution of 10 - 50 percent by weight at temperatures not exceeding the boiling point of the alkaline solution.