Verfahren zum Regenerieren von Katalysatoren auf Wismutmolybdat- und Wismutwolframat-Basis
Heat-degraded bismuth-containing catalysts are regenerated by contact with concentrated ammonium hydroxide. Contact may be by immersing or slurrying the catalyst in NH4OH or causing the reagent to flow over the catalyst. The catalyst may be supported on SiO2, Al2O3 or ball clay. Additionally the cat...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Heat-degraded bismuth-containing catalysts are regenerated by contact with concentrated ammonium hydroxide. Contact may be by immersing or slurrying the catalyst in NH4OH or causing the reagent to flow over the catalyst. The catalyst may be supported on SiO2, Al2O3 or ball clay. Additionally the catalyst may contain one of Mo, Cu, P, Si, S. Fe, Sn, Pb, As, Sb, Ag, Te and Co. |
---|