Feuerfeste Materialien und Ofenauskleidungen
A fused cast refractory consists of at least 80% by weight of MgO + CaO + BaO + SrO, the amount of MgO being at least 50% and the total of CaO + BaO + SrO being less than 35%, and 0.05-20% of fluorine wherein when the MgO content is 50-80% the refractory may also contain 0-6% Al2O3, 0-4% SiO2, 0-8%...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | ger |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A fused cast refractory consists of at least 80% by weight of MgO + CaO + BaO + SrO, the amount of MgO being at least 50% and the total of CaO + BaO + SrO being less than 35%, and 0.05-20% of fluorine wherein when the MgO content is 50-80% the refractory may also contain 0-6% Al2O3, 0-4% SiO2, 0-8% TiO2, 0-10% ZrO2, the total of these oxides being 0-10%, and 0-10% of FeO and when the MgO content is at least 80% the total of CuO + BaO + SrO is less than 19% and the refractory may also contain 0-10% Al2O3, 0-18% Cr2O3, 0-8% SiO2, 0-12% TiO2, 0-15% ZrO2 and 0-10% of FeO. The fluorine may be added as calcium or magnesium fluoride. Fusion temperatures of 2000-2800 DEG C. are specified. Specifications 265,847 and 950,393 are referred to. |
---|