Verfahren zur Herstellung eines modifizierten Olefinpolymers

A process for producing a modified olefin polymer includes the steps of: (1) blending 100 parts by weight of an olefin polymer, 0.01 to 20 parts by weight of a polar group-carrying unsaturated compound, and 0.001 to 20 parts by weight of an organic peroxide, with one another, in a continuous extrude...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKEI, TSUYOSHI, TSUKUI, HITOSHI
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A process for producing a modified olefin polymer includes the steps of: (1) blending 100 parts by weight of an olefin polymer, 0.01 to 20 parts by weight of a polar group-carrying unsaturated compound, and 0.001 to 20 parts by weight of an organic peroxide, with one another, in a continuous extruder at a temperature T1 for a time S1, thereby forming a first blend; (2) blending the first blend in the continuous extruder at a temperature T2 for a time S2, thereby forming a second blend; and (3) blending the second blend in the continuous extruder at a temperature T3 for a time S3. T1, T2 and T3 have specific relationships to decomposition temperatures of the organic peroxide, and S1, S2 and S3 have specific relationships to half-lives of the organic peroxide.