Propylene based polymer useful for the production of stretched film for packaging, has defined melt index, m.pt. and half height width of the DSC melt peak

A propylene based polymer has a melt index (JIS K7210) of 1.0-20 g/10 min) and a m.pt. (Tm) measured using a differential scanning calorimeter (DSC) of 147-159 deg C in which the half-height width (HW) of the melt peak as measured by DSC is characterized. A propylene based polymer (I) has a melt ind...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YUNOKI, SYUNJI, TSUJI, MITSUJI, YADA, KENICHIRO
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A propylene based polymer has a melt index (JIS K7210) of 1.0-20 g/10 min) and a m.pt. (Tm) measured using a differential scanning calorimeter (DSC) of 147-159 deg C in which the half-height width (HW) of the melt peak as measured by DSC is characterized. A propylene based polymer (I) has a melt index (JIS K7210) of 1.0-20 g/10 min) and a m.pt. (Tm) measured using a differential scanning calorimeter (DSC) of 147-159 deg C in which the half-height width (HW) of the melt peak as measured by DSC is characterized by equation (1). HW