A fire-free brick is prepared from cement (9-11 Wt portions), self-burning coal gangue (45-50), grain slag (15-30), stone powder (20-30), water reducing agent (0.2) and sodium sulfate (0.21). Its advantages are high quality, low cost and no environmental pollution.